Атауы: Standard Guide for Crevice Corrosion Testing of Iron-Base and Nickel-Base Stainless Alloys in Seawater and Other Chloride-Containing Aqueous Environments
Белгілеу: ASTM G78 - 20 (2025)
Санат: ASTM
МСЖ: 07.030
Беттер саны: 7
Әзірлеуші: ASTM
Мәртебе: Дата введения в БД
Тіркелген күні: 01.08.2025
Бұйрық: Английский
Тіл: Английский (США)
Кілт сөздер: aqueous; chloride; corrosion; crevice; iron-base; nickel-base; testing
Аннотация: Crevice corrosion of iron-base and nickel-base stainless alloys can occur when an occlusion or crevice limits access of the bulk environment to a localized area of the metal surface. Localized environmental changes in this stagnant area can result in the formation of acidic/high chloride conditions that may result in initiation and propagation of crevice corrosion of susceptible alloys. In practice, crevices can generally be classified into two categories: (1) naturally occurring, that is, those created by biofouling, sediment, debris, deposits, etc., and (2) man-made, that is, those created during manufacturing, fabrication, assembly, or service. Crevice formers utilized in laboratory and field studies can represent actual geometric conditions encountered in some service applications. Use of such crevice formers in service-type environments are not considered accelerated test methods. The geometry of a crevice can be described by the dimensions of crevice gap and crevice depth. Crevice gap is identified as the width or space between the metal surface and the crevice former. Crevice depth is the distance from the mouth to the center or base of the crevice.
Замененные: -
Заменяющие: -
Принадлежность к ТР ТС: -
Жаңарту күні: 01.08.2025
Жаңарту мәтіні: В соответствии с статьей 27 ЗРК "О стандартизации"
ASTM G78 - 20 (2025). Standard Guide for Crevice Corrosion Testing of Iron-Base and Nickel-Base Stainless Alloys in Seawater and Other Chloride-Containing Aqueous Environments
ГОСТ ISO 8909-3-2025ГОСТ